将锡合金焊料挤压成¢9毫米、¢12毫米、¢15毫米的焊丝,助焊剂含量为2.5%±0.1%。

Heats tin alloy solder to 300-400°C, casts into 0.5 kg or 1.0 kg bars.  

Melts leaded and lead-free solder products, including tin-based alloys.

Separates lead-tin alloys with >80% tin, achieving 99.98% tin purity.  

Processes lead-free solder wire, finest ¢1.5 mm, efficiency 150~200 kg/hour;Processes leaded solder wire, finest ¢2.2 mm, efficiency 200 kg/hour.

以锡锭为原料,生产电镀锡阳极半球。采用低压浇铸,表面光滑美观。  

< 1234 >